Abstract

The high chromium, molybdenum, and nitrogen contents of alloy UR 2507W (PREN ≥ 40) explain why the grade is very resistant to localized corrosion even in acidified oxidizing environments. The alloy has been used for offshore applications. This datasheet provides information on composition, physical properties, elasticity, tensile properties, and shear strength. It also includes information on corrosion resistance as well as forming, heat treating, and joining. Filing Code: SS-1202. Producer or source: Industeel USA, LLC.