Abstract

Lescalloy HY-180 VIM-VAR is a clean high-strength alloy steel with high strength and very high fracture toughness. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as fracture toughness. It also includes information on forming and heat treating. Filing Code: SA-719. Producer or source: Latrobe Specialty Steel Company.