Abstract
NSSMC-NAR-301L HS1 is an austenitic stainless steel with excellent corrosion resistance. This datasheet provides information on composition, hardness, and tensile properties as well as fatigue. It also includes information on forming. Filing Code: SS-1232. Producer or source: Nippon Steel and Sumitomo Metal Corporation.