Ancorsteel DWP200 is a water-atomized low apparent density powder for structural applications. The atomizing process imparts a more irregular spongy morphology to the powder particles, giving DWP200 a superior combination of green strength and compressibility compared to other atomized powders. This datasheet provides information on composition, physical properties, microstructure, tensile properties. It also includes information on powder metal forms. Filing Code: CS-192. Producer or source: Hoeganaes Corporation.