Abstract

Kubota alloy KHR35AF is a heat resisting wholly austenitic stainless steel casting for ethylene pyrolysis. This datasheet provides information on composition, physical properties, elasticity, tensile properties, and shear strength as well as creep. It also includes information on casting and joining. Filing Code: SS-1184. Producer or source: Kubota Metal Corporation.