Abstract

MX01 is a steel grade developed to achieve useful properties to minimize the cost of forging dies. This datasheet provides information on composition, hardness, and tensile properties as well as fracture toughness. It also includes information on forming. Filing Code: SA-708. Producer or source: Industeel USA, LLC.