BrushForm 96 strip is a high-performance, heat treatable spinodal copper-nickel-tin alloy designed to provide optimal formability and strength characteristics in conductive spring applications. It is available in both pre-heat treated (mill hardened) and heat treatable (age hardenable) forms. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. and bend strength. It also includes information on forming. Filing Code: Cu-833. Producer or source: Materion Brush Performance Alloys.