Abstract

Sandvik Sanicro 36Mo is a corrosion resistant grade (CRA) available as wire for service in extremely sour oil and gas wells. This datasheet provides information on composition, physical properties, and elasticity. It also includes information on corrosion resistance as well as forming. Filing Code: SS-1172. Producer or source: Sandvik Steel Company.