MA276 is a Ni-16Cr-16Mo-5Fe-4W (mass %) nickel-base corrosion-resistant alloy superior in a wide range of corrosive environments. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as fracture toughness. It also includes information on low and high temperature performance, and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Ni-711. Producer or source: MMC Superalloy Corporation.