Sandvik Sanicro 29 is a corrosion resistant grade (CRA) available as seamless product heavily cold worked for oil country tubular applications at high strengths. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on corrosion resistance as well as forming and heat treating. Filing Code: SS-1169. Producer or source: Sandvik Steel Company.