XAR 600 is a wear-resistant structural steel as heavy plate that is water quenched. It has very good abrasion resistance. Hardness in the quenched and tempered condition is greater than 550 HBW. This datasheet provides information on composition, hardness, and tensile properties as well as fracture toughness. It also includes information on forming, heat treating, machining, and joining. Filing Code: SA-696. Producer or source: ThyssenKrupp Steel Europe AG.