Docol 1000 LCE is a high-strength steels with a microstructure that contains ferrite, which is soft and contributes to good formability, and martensite, which is hard and contributes to the strength of the material. These steels are designed according to their lowest tensile strength. This datasheet provides information on composition, physical properties, tensile properties, and bend strength. It also includes information on forming and joining. Filing Code: SA-694. Producer or source: SSAB Swedish Steel Inc.. See also Alloy Digest SA-615, March 2010.