Abstract

Timetal 7-4 is an alpha + beta alloy with excellent creep resistance and high strength. This datasheet provides information on composition, physical properties, and tensile properties as well as creep. It also includes information on forming. Filing Code: Ti-151. Producer or source: Timet.