Sandvik SanRig 80, an austenitic stainless steel, has high fatigue and tensile strength for marine applications. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as fatigue. It also includes information on corrosion resistance as well as forming. Filing Code: SS-1168. Producer or source: Sandvik Steel Company.