Abstract
Quend 700 is an extra-high-strength structural steel for mining and earth moving equipment. It has a minimum yield strength of 700 MPa (102 ksi). This datasheet provides information on composition and tensile properties as well as fracture toughness. It also includes information on forming, heat treating, machining, and joining. Filing Code: SA-693. Producer or source: NLMK Clabecq.