Nioro ABA is a gold/nickel-based brazing alloy for ceramics. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on forming and joining. Filing Code: Au-3. Producer or source: Morgan Advanced Materials plc.