Abstract
Ansonia alloy ACB C18900 was developed to be able to make the finest welds possible in copper. This datasheet provides information on composition, physical properties, and tensile properties. It also includes information on forming, heat treating, and joining. Filing Code: Cu-830. Producer or source: Ansonia Copper & Brass Inc..