Böhler (or Boehler) W403 VMR is a tool steel with outstanding properties, based not only on a modified chemical composition, but on the selection of highly clean raw materials for melting, remelting under vacuum (VMF), optimized diffusion annealing, and a special heat treatment. This datasheet provides information on composition, physical properties, and elasticity. It also includes information on forming and heat treating. Filing Code: TS-721. Producer or source: Böhler Edelstahl GmbH.