Dillidur 500V is a water hardened wear-resistant steel with surface hardness at room temperature of 310-370 HB. It has a high resistance to abrasion and impact wear in combination with good welding performance. This steel is used in the production of excavator buckets, stone crushers, and loading machines. This datasheet provides information on composition, physical properties, hardness, and tensile properties as well as fracture toughness. It also includes information on wear resistance as well as forming, heat treating, machining, and joining. Filing Code: SA-681. Producer or source: Dillinger Hütte GTS.