DIMO 2738 is a prehardened CrMnNiMo alloyed tool steel for construction of plastic molds. This datasheet provides information on composition, physical properties, and hardness. It also includes information on forming and heat treating. Filing Code: TS-720. Producer or source: AG der Dillinger Hüttenwerke.