Armox 500T combines good ballistic properties with excellent toughness. Hardness is 480–540 HBW. This datasheet provides information on composition, tensile properties, and bend strength as well as fracture toughness. It also includes information on forming and joining. Filing Code: SA-680. Producer or source: SSAB Armox.