Abstract

Centralloy HT E is a cast nickel alloy with very good high-temperature properties. This datasheet provides information on composition and tensile properties. It also includes information on casting, machining, and joining. Filing Code: Ni-709. Producer or source: Schmidt & Clemens Inc..