Abstract

Centralloy H101 Micro is a cast austenitic stainless alloy with very good high temperature properties. The alloy has carbides in a uniform dispersion that impedes dislocation movement. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on casting, machining, and joining. Filing Code: SS-1148. Producer or source: Schmidt & Clemens Inc..