Abstract

Supralsim 690 QL1 is a high yield-strength quenched and tempered steel for welded and weight-saving structures. This datasheet provides information on composition and tensile properties as well as fracture toughness. It also includes information on forming, machining, and joining. Filing Code: SA-678. Producer or source: Industeel USA, LLC.