MoldMAX V is a high conductivity, moderately high strength, copper-nickel-silicon-chromium alloy. The alloy has a unique combination of thermal conductivity and strength. The MoldMAX copper mold alloys provide short cycle times, plastic part dimensional control, parting line maintenance, and good corrosion resistance This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness and fatigue. It also includes information on corrosion and wear resistance as well as forming, machining, joining, and surface treatment. Filing Code: Cu-822. Producer or source: Materion Brush Performance Alloys.