Abstract

Märker WM 28 is an all-purpose hot-working tool steel with very good hot strength. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as creep. It also includes information on heat treating. Filing Code: TS-717. Producer or source: Schmidt & Clemens Inc..