Abstract

Mueller Alloy C27450 has excellent machining characteristics for forged and machined applications required to meet AB1953. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on forming, heat treating, and machining. Filing Code: Cu-820. Producer or source: Mueller Industries.