Abstract

ToughMet 2 CX is a Cu-9Ni-6Sn alloy that combines low coefficient of friction with wear resistance. ToughMet alloys are a line of spinodal hardened Cu-Ni antigalling alloys for bearings capable of performing with a variety of shafting materials and lubricants. The alloys combine a high lubricity with wear resistance in these severe loading conditions. ToughMet 2CX in the cast and spinodally hardened (CX) condition exhibits tensile strength in excess of 724 MPa (105 ksi) and hardness exceeding HRC 27 with excellent machinability. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming. Filing Code: Cu-819. Producer or source: Materion Brush Performance Alloys.