Abstract

TYPLEX is a hot work tool steel with nickel to improve toughness. This datasheet provides information on composition, physical properties, hardness, and elasticity as well as fracture toughness. It also includes information on wear resistance as well as heat treating. Filing Code: TS-716. Producer or source: Latrobe Specialty Steel Company.