Abstract

Mueller Alloy C37700 has excellent machining characteristics that make it useful for general forging applications. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on forming, heat treating, machining, and joining. Filing Code: Cu-817. Producer or source: Mueller Industries.