Abstract

NAS 75N is a super duplex stainless steel with a very high PRE number. This datasheet provides information on composition, physical properties, hardness, and tensile properties as well as fracture toughness. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, and joining. Filing Code: SS-1140. Producer or source: Nippon Yakin Kogyo Company Ltd.