CryElso 9Q is a steel alloy for extra low temperature applications and requiring high impact values. This datasheet provides information on composition, tensile properties, and shear strength as well as fracture toughness. It also includes information on low temperature performance as well as forming, heat treating, and joining. Filing Code: SA-673. Producer or source: Industeel USA, LLC.