Abstract

MARS 300 is a super high-hardness (620 HB) steel for ballistic protection. This datasheet provides information on composition, physical properties, hardness, and tensile properties as well as fracture toughness. It also includes information on forming, heat treating, machining, and joining. Filing Code: SA-685. Producer or source: Industeel USA, LLC and Industeel France.

This content is only available as a PDF.
You do not currently have access to this content.