Abstract
LSS 2367 is a European designation DIN 1.2367 and is similar to AISI H11. This datasheet provides information on composition, physical properties, and hardness. It also includes information on wear resistance as well as heat treating and machining. Filing Code: TS-723. Producer or source: Latrobe Specialty Steel Company.