Abstract

Böhler (or Boehler) W405 is a hot work steel with a great combination of hardness, strength, toughness, ductility, and thermal conductivity to resist typical damage mechanisms in applications. This datasheet provides information on composition, physical properties, and elasticity. It also includes information on forming and heat treating. Filing Code: TS-722. Producer or source: Böhler-Uddeholm North America.