LSS H21 is a hot work tool steel recommended for difficult hot work tooling applications. This datasheet provides information on composition, physical properties, hardness, and elasticity as well as fracture toughness. It also includes information on heat treating and machining. Filing Code: TS-713. Producer or source: Latrobe Specialty Steel Company.