Abstract

Inconel Filler Metal 52MSS contains about 2.0–2.5 wt.% Nb and 3.0–4.0 wt% Mo, which have been shown to improve resistance to ductility dip cracking, and has reduced aluminum and titanium, which provide the ability to deposit very clean weld deposits without the floating oxide impurities of other previously used filler metals. This datasheet provides information on composition and tensile properties. It also includes information on forming, heat treating, and joining. Filing Code: Ni-706. Producer or source: Special Metals Welding Products Corporation.