Böhler (or Boehler) L359 is a nickel-base alloy with good resistance to stress-corrosion cracking, and excellent corrosion resistance to all types of nonuniform corrosion. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on high temperature performance as well as forming, heat treating, and joining. Filing Code: Ni-700. Producer or source: Böhler-Uddeholm North America.