Abstract

Wieland-K62 is a high conductivity alloy for a variety of electronic and electrical applications. This datasheet provides information on composition, physical properties, elasticity, tensile properties, and bend strength. It also includes information on corrosion resistance as well as forming, machining, and joining. Filing Code: Cu-812. Producer or source: Wieland Metals Inc..