Böhler (or Boehler) L359 is a nickel base alloy with good resistance to chloride attack. The alloy is used for handling a wide range of corrosive media. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as fracture toughness. It also includes information on high temperature performance as well as forming, heat treating, and joining. Filing Code: Ni-698. Producer or source: Böhler-Uddeholm North America.