Abstract

Crucible CPM Rex 66 is a high-speed tool steel of the tungsten type made by the CPM process. This datasheet provides information on composition, physical properties, microstructure, hardness, and elasticity. It also includes information on heat treating and machining. Filing Code: TS-704. Producer or source: Crucible Industries LLC.