Formadur PH X Superclean is a corrosion-resistant, precipitation-hardened steel with high strength. It shows excellent polishability due to the applied remelting process. Compared to Formadur 2316, hardness in as-delivered condition and corrosion resistance are improved. This datasheet provides information on composition, physical properties, hardness, and tensile properties as well as fracture toughness. It also includes information on corrosion resistance as well as heat treating, machining, and joining. Filing Code: SS-1122. Producer or source: Schmolz + Bickenbach.