Abstract

Abrazo 450 is roller quenched to obtain high strength, good properties, and excellent wear resistance. This datasheet provides information on composition, physical properties, hardness, and tensile properties as well as fracture toughness. It also includes information on forming. Filing Code: SA-651. Producer or source: Corus Long Products.