NAS 825 is a corrosion-resistant nickel alloy that has resistance to both oxidizing and reducing environments, and with 42% nickel, the alloy is very resistant to chloride-ion stress-corrosion cracking. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Ni-694. Producer or source: Nippon Yakin Kogyo Company Ltd.