Abstract
Cryodur 1520 is a shell-hardenable steel with wear resistance. This datasheet provides information on composition, physical properties, and hardness. It also includes information on wear resistance as well as heat treating. Filing Code: TS-711. Producer or source: Schmolz + Bickenbach USA Inc..