Formadur 2316 is a plastic mold steel (modified Type 420) with good polishability. It is used for molds for processing plastics with corrosive reactions. This datasheet provides information on composition, physical properties, and hardness. It also includes information on heat treating. Filing Code: TS-710. Producer or source: Schmolz + Bickenbach USA Inc..