Abstract

MARS 220 is a medium hardness steel (440 HB) for blast protection. This datasheet provides information on composition, physical properties, hardness, tensile properties, and bend strength as well as fracture toughness. It also includes information on forming, heat treating, and joining. Filing Code: SA-667. Producer or source: Industeel USA, LLC.