Abstract
Ancorsteel 1015 alloy is a low apparent density water-atomized alloy. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on powder metal forms. Filing Code: CS-171. Producer or source: Hoeganaes Corporation.