ATI Ti-5Al-2Sn-2Zr-4Cr-4Mo is known as Ti-17 alloy and is a beta-rich material for large aerospace components. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, and joining. Filing Code: Ti-149. Producer or source: ATI Allvac.