Dillidur 500V is a water hardened wear-resistant steel with surface hardness at room temperature of 470-530 HB. It has the highest wear resistance of the Dillidur steels. It is used in the production of transport systems, earth-moving plants, recycling plants, and stone crushers. This datasheet provides information on composition, physical properties, hardness, and tensile properties as well as fracture toughness. It also includes information on wear resistance and surface qualities as well as forming, heat treating, machining, and joining. Filing Code: SA-641. Producer or source: Dillinger Hütte GTS.